Give good protection against oxidative heat ageing, anti flex cracking. no conversion of insoluble sulphur to soluble sulphur on storage in green compound. hence avoid any possibility of sulphur blooming thus not impairing tack, better adhesion. better performance in bonding compounds for rubber composite (tires, belting, hoses) with fabric/cord, steel cord/wire. hot retread compounds for otr & tractor tires.
Cushion Gum Compounds.
Description | Unit | Nominal Value |
---|---|---|
FTIR correlation with reference | % | 98 min. |
Specific Gravity by Bottle at 25ºC | N / A | 1.30 ± 0.05 |
Ash Content (at 750ºC for 2 hrs.) | % W / W | 30.50 ± 2.50 |
Acetone Extract | % W / W | 65.00 Min |
Moisture content (Azeotropic reflux) | % W / W | 2.0 Max |
Heat loss (105°C/1hr.) | % W / W | 3.0 Max |
These raw material properties are typical properties and, unless specifically indicated otherwise, are not to be considered as delivery specification.
25 Kgs paper bags
1 year from the date of production if stored properly in original packing at ambient temperature.